| Share |
|
Please use this identifier to cite or link to this item:
https://tede.unioeste.br/handle/tede/8747| Tipo do documento: | Dissertação |
| Title: | Efeito do gás ozonizado em diferentes concentrações sob a resistência de união adesiva em dentina por microtração: Estudo in vitro com um sistema adesivo universal |
| Other Titles: | Effect of ozonated gas at different concentrations on the adhesive bond strength to dentin via microtensile testing: an in vitro study using a universal adhesive system |
| Autor: | Vincenzi, Carlos Francisco |
| Primeiro orientador: | Mendonça, Marcio José |
| Primeiro coorientador: | Camilotti, Veridiana |
| Primeiro membro da banca: | Mendonça, Marcio José |
| Segundo membro da banca: | Bosquiroli, Virginia |
| Terceiro membro da banca: | Silva, Emanuely da ![]() |
| Resumo: | Introdução: A aplicação de ozônio tem sido proposta como método complementar de tratamento da superfície dentinária previamente aos procedimentos adesivos. Objetivo: Avaliar, in vitro, o efeito de diferentes tratamentos da superfície dentinária sobre a resistência de união à microtração, comparando água destilada, água ozonizada e gás ozonizado nas concentrações de 20, 30 e 40 µg/mL. Metodologia: Cinquenta e cinco terceiros molares humanos foram distribuídos aleatoriamente em cinco grupos experimentais (n=11): água destilada – controle (AD), água ozonizada (AO), gás ozonizado a 20 µg/mL (O20), 30 µg/mL (O30) e 40 µg/mL (O40). Após os respectivos tratamentos, foi aplicado um sistema adesivo universal e confeccionado um bloco de resina composta. Após sete dias de armazenamento, as amostras foram seccionadas em corpos de prova e submetidas ao teste de resistência de união à microtração (µTBS). Os padrões de fratura foram classificados como adesivo, misto, coesivo em resina ou coesivo em dentina. A distribuição dos dados foi avaliada pelo teste de Shapiro-Wilk e as comparações entre os grupos foram realizadas pelo teste de Kruskal-Wallis, seguido pelo teste de Dunn, adotando-se nível de significância de 5%. Resultados: O grupo O20 apresentou a maior média de resistência de união (18,26 ± 3,57 MPa), seguido pelos grupos Controle (16,09 ± 2,28 MPa), O40 (15,82 ± 2,75 MPa), O30 (13,42 ± 3,08 MPa) e AO (12,95 ± 4,38 MPa). O teste de Kruskal-Wallis indicou diferença estatisticamente significativa entre os tratamentos (p<0,05). Conclusão: Nas condições experimentais avaliadas, o grupo O20 apresentou o maior valor médio de resistência de união. Entretanto, os resultados não permitem estabelecer superioridade geral dessa concentração em relação aos demais protocolos, e o aumento da concentração do gás ozonizado não foi acompanhado por aumento progressivo da resistência de união. |
| Abstract: | Introduction: Ozone application has been proposed as a complementary approach for dentin surface treatment prior to adhesive restorative procedures. Objective: To evaluate, in vitro, the effect of different dentin surface treatments on microtensile bond strength by comparing distilled water, ozonated water, and ozonated gas at concentrations of 20, 30, and 40 µg/mL. Methods: Fifty-five human third molars were randomly distributed into five experimental groups (n = 11): distilled water – control group (DW), ozonated water (OW), ozonated gas at a concentration of 20 µg/mL (O20), ozonated gas at 30 µg/mL (O30), and ozonated gas at 40 µg/mL (O40). After the respective dentin surface treatments, a universal adhesive system was applied, followed by the build-up of a composite resin block. After a seven-day storage period, the samples were sectioned into stick-shaped specimens, which were subjected to the microtensile bond strength test (µTBS), with the results expressed in MPa. Failure patterns were subsequently analyzed and classified as adhesive, mixed, cohesive in composite resin, or cohesive in dentin. Data distribution was assessed using the Shapiro Wilk test, and comparisons among the experimental groups were performed using the Kruskal-Wallis test followed by Dunn’s multiple-comparison test, adopting a significance level of 5%. Results: The O20 group showed the highest mean microtensile bond strength (18.26 ± 3.57 MPa), followed by the Control group (16.09 ± 2.28 MPa), O40 (15.82 ± 2.75 MPa), O30 (13.42 ± 3.08 MPa), and OW (12.95 ± 4.38 MPa). The Kruskal-Wallis test indicated a statistically significant difference among the experimental treatments (p < 0.05). Thus, although the O20 group exhibited the highest numerical mean bond strength, the statistical findings should be considered when interpreting the performance of the different treatment protocols. Conclusion: Under the experimental conditions evaluated in this study, the O20 group showed the highest mean bond strength to dentin. However, the results do not support establishing an overall superiority of this concentration over the other experimental protocols. Furthermore, increasing the ozonated gas concentration from 20 to 30 and 40 µg/mL was not accompanied by a progressive increase in bond strength. |
| Keywords: | Ozônio Resinas compostas Adesivos Dentinários Resistência à Tração Ozone Composite resins Dentin-bonding agents Tensile strength |
| CNPq areas: | Odontologia |
| Idioma: | por |
| País: | Brasil |
| Publisher: | Universidade Estadual do Oeste do Paraná |
| Sigla da instituição: | UNIOESTE |
| Departamento: | Centro de Ciências Biológicas e da Saúde |
| Program: | Programa de Pós-Graduação em Odontologia |
| Campun: | Cascavel |
| Citation: | VINCENZI, Carlos Francisco. Efeito do gás ozonizado em diferentes concentrações sob a resistência de união adesiva em dentina por microtração: Estudo in vitro com um sistema adesivo universal. 2026. 27 f. Dissertação (Mestrado em Odontologia) - Universidade Estadual do Oeste do Paraná, Cascavel. |
| Tipo de acesso: | Acesso Aberto |
| Endereço da licença: | http://creativecommons.org/licenses/by-nc-nd/4.0/ |
| URI: | https://tede.unioeste.br/handle/tede/8747 |
| Issue Date: | 26-Aug-2026 |
| Appears in Collections: | Mestrado em Odontologia (CVL) |
Files in This Item:
| File | Description | Size | Format | |
|---|---|---|---|---|
| Carlos Francisco Vincenzi.pdf | 821.76 kB | Adobe PDF | View/Open Preview |
Items in TEDE are protected by copyright, with all rights reserved, unless otherwise indicated.